Orange peel

10/13/2021 2:30:06 PM
(0)
(0)

Orange peel

Orange peel

Orange peel

Cause

• Incorrect spraying pressure or viscosity, spraying technique or application temperature

• Unsuitable combination of solvents or low quality solvents

• Insufficient sanding of substrate

• Incorrect spray gun set up

• Excessive temperature

spray,viscosity,technique,low,quality,solvent,sustrate,temperature,application,sand,substrate,thinner,hardner

 

Prevention

• Follow application recommendations from technical data sheets

• Prepare and sand substrate correctly

• Use recommended gun set up

• Always use recommended thinners

• Avoid application at very high temperatures

 

 

Remedy

• Sand and repaint

• Sand and polish